Cast iron is always a challenge. This part was pre-heated to 500F and stick welded with
1/8 inch 55% nickel electrode. The part was then cooled slowly to room temperature over a period of 2 hours. I used TIG with a stainless rod for the smaller clamp, same preheat and cooling applies.